Copper Sheet

Short Description:

Copper Sheet is made of electrolytic copper, through processing by ingot, hot rolling, cold rolling, heat treatment, surface cleaning, cutting, finishing, and then packing.


Product Detail

Product Tags

Product Introduction

Copper Sheet is made of electrolytic copper, through processing by ingot, hot rolling, cold rolling, heat treatment, surface cleaning, cutting, finishing, and then packing. The material has excellent thermal and electrical conduction, flexible ductility and good corrosion resistance. It has been widely used in electrical, automotive, communications, hardware, decoration and other industries. 

Main Technical Parameters

1-1 Chemical Composition

Alloy

No.

Chemical Composition (%Max.)

Cu+Ag

P

Bi

Sb

As

Fe

Ni

Pb

Sn

S

Zn

O

Impurity

T1

99.95

0.001

0.001

0.002

0.002

0.005

0.002

0.003

0.002

0.005

0.005

0.02

0.05

T2

99.90

---

0.001

0.002

0.002

0.005

0.005

0.005

0.002

0.005

0.005

0.06

0.1

TU1

99.97

0.002

0.001

0.002

0.002

0.004

0.002

0.003

0.002

0.004

0.003

0.002

0.03

TU2

99.95

0.002

0.001

0.002

0.002

0.004

0.002

0.004

0.002

0.004

0.003

0.003

0.05

TP1

99.90

---

0.002

0.002

---

0.01

0.004

0.005

0.002

0.005

0.005

0.01

0.1

TP2

99.85

---

0.002

0.002

---

0.05

0.01

0.005

0.01

0.005

---

0.01

0.15

1-2 Alloy Table

Name

China

ISO

ASTM

JIS

Pure Copper

T1,T2

Cu-FRHC

C11000

C1100

oxygen-free copper

TU1

------

C10100

C1011

TU2

Cu-OF

C10200

C1020

deoxidized copper

TP1

Cu-DLP

C12000

C1201

TP2

Cu-DHP

C12200

C1220

1-3 Features

1-3-1Specification mm

Name

Alloy(China)

Temper

Size(mm)

Thickness

Width

Length

Copper Sheet

T2/TU2

H  1/4H
1/2H  H

0.3~0.49

600

1000~2000

0.5~3.0

600~1000

1000~3000

Temper Mark:O. Soft;1/4H. 1/4 Hard;1/2H. 1/2 Hard;H. Hard;EH. Ultrahard;R. Hot Rolled.

1-3-2 Tolerance Unit: mm

Thickness

Width

Thickness Allow Deviation±

Width Allow Deviation±

<400

<600

<1000

<400

<600

<1000

0.5~0.8

0.035

0.050

0.080

0.3

0.3

1.5

0.8~1.2

0.040

0.060

0.090

0.3

0.5

1.5

1.2~2.0

0.050

0.080

0.100

0.3

0.5

2.5

2.0~3.2

0.060

0.100

0.120

0.5

0.5

2.5

1-3-3 Mechanical Performance:

Alloy

Temper

Tensile Strength N/mm2

Elongation

%

Hardness

HV

T1

T2

M

(O)

205-255

30

50-65

TU1

TU2

Y4

(1/4H)

225-275

25

55-85

TP1

TP2

Y2

(1/2H)

245-315

10

75-120

 

 

Y

(H)

≥275

3

≥90

Temper Mark:O. Soft;1/4H. 1/4 Hard;1/2H. 1/2 Hard;H. Hard;EH. Ultrahard;R. Hot Rolled.

1-3-4 Electrical Parameters:

Alloy

Conductivity/%IACS

Resistance Coefficient /Ωmm2/m

T1  T2

≥98

0.017593

TU1 TU2

≥100

0.017241

TP1 TP2

≥90

0.019156

1-3-4 Electrical Parameters

2